Synthesis of ZnO/PMMA nanocomposite by low-temperature atomic layer deposition for possible photocatalysis applications
Publication date: 1 November 2020Source: Materials Science in Semiconductor Processing, Volume 118Author(s): Alessandro Di Mauro, Clayton Farrugia, Stephen Abela, Paul Refalo, Maurice Grech, Luciano Falqui, Vittorio Privitera, Giuliana Impellizzeri
Source: Materials Science in Semiconductor Processing - Category: Materials Science Source Type: research