Comparison of color changes, fracture strengths, and failure modes of conventional endocrowns and endocrowns with different design modifications

CONCLUSION: The recorded Δ⁢E values of ECs in all groups were equal or marginally higher than the acceptable values. The EC with a 3 mm chamfer and ferrule displayed the highest mean maximum load. The EC with a 5 mm chamfer finish line had a marginally lower maximum load at fracture than other ECs. Failures, such as ceramic fracture, split fracture, and ceramic and tooth splitting above the cemento-enamel junction (CEJ) or vertically were predominant in samples with occlusal preparation depths of 3 mm with ferrule and 5 mm.PMID:38427513 | DOI:10.3233/THC-231175
Source: Technology and Health Care - Category: Medical Devices Authors: Source Type: research