Compressive behavior and elastic properties of Ni-based γ/γ’ ternary model superalloys: First-principles calculations and rule of mixtures predications
Publication date: 25 October 2020Source: Journal of Alloys and Compounds, Volume 839Author(s): Minru Wen, Xing Xie, Huafeng Dong, Zhiping Lin, Fugen Wu, Chong-Yu Wang