Assessment of the marginal fit, ceramo-metal shear bond strength and the fractographic analysis of sinter cast gold: An In-vitro study
Conclusion: The marginal fit observed before and after ceramic firing was within clinically acceptable range, whereas the ceramo-metal shear bond strength between sinter cast gold and ceramic was found to be inadequate.
Source: Journal of Orofacial Sciences - Category: Dentistry Authors: Hetal Turakhia Sabita M Ram Aruna Mehta Abhishek S Nayyar Source Type: research