Integrated TEM/transmission-EBSD for recrystallization analysis in nickel-based disc superalloy
Publication date: Available online 27 November 2020Source: Progress in Natural Science: Materials InternationalAuthor(s): Fei Sun
Source: Progress in Natural Science: Materials International - Category: Materials Science Source Type: research