Synthesis, microstructural characterization and nanoindentation of Zr, Zr-nitride and Zr-carbonitride coatings deposited using magnetron sputtering
Publication date: Available online 25 November 2020Source: Journal of Advanced ResearchAuthor(s): Anwar Ul-Hamid
Source: Journal of Advanced Research - Category: Research Source Type: research
More News: Nanotechnology | Research