Effects of Khat on Surface Roughness and Color of Feldspathic and Zirconia Porcelain Materials under Simulated Oral Cavity Conditions.
Conclusion: KH significantly affected both surface parameter and color of glazed or polished porcelain materials and natural teeth.
PMID: 32414190 [PubMed - in process]
Source: Medicina (Kaunas) - Category: Universities & Medical Training Authors: Moaleem MMA, AlSanosy R, Ahmari NMA, Shariff M, Alshadidi AA, Alhazmi HA, Khalid A Tags: Medicina (Kaunas) Source Type: research