Fracture rate of 188695 lithium disilicate and zirconia ceramic restorations after up to 7.5 years of clinical service: A dental laboratory survey

ConclusionsWithin the 7.5-year period, restorations fabricated with lithium disilicate and zirconia restorations had relatively low fracture rates. Monolithic restorations fractured at a lower rate than layered restorations.