Immobilisation of high-arsenic-containing tailings by using metallurgical slag-cementing materials.

In this study, these cementitious materials were combined with high-arsenic-containing tailings to form cemented backfill material (CBM). The results indicated that the optimal design of CBM was that of specimen CBM2 which showed good early strength (10.09 MPa) at a curing age of 3 days containing 60% BF slag, 30% SS, and 10% gypsum. And the arsenic leaching concentration of CBM2 at a curing age of 7 days and 28 days were both less than the limits specified in standards for drinking water quality (Chinese Standard GB 5749-2006). The predominant hydration products of CBM2 contained rod-like ettringite and amorphous C-S-H gel both of which promote arsenic solidification. PMID: 30772590 [PubMed - indexed for MEDLINE]