Fracture resistance and failure modes of lithium disilicate or composite endocrowns
Conclusions: The lithium disilicate ceramic endocrowns exhibited higher fracture resistance than indirect composite groups. Both of the composite endocrowns showed more favorable failure than the lithium disilicate ceramic endocrowns.
Source: Nigerian Journal of Clinical Practice - Category: Rural Health Authors: M Altier F Erol G Yildirim EE Dalkilic Source Type: research