Adhesive performance of precoated brackets after expiration.
CONCLUSIONS: Adhesive precoated brackets did not have any reduction in enamel-adhesion properties up to 4 years after their expiration date. Extended shelf life testing for precoated dental brackets may be worth considering.
PMID: 26172317 [PubMed - as supplied by publisher]